Environmental stress corrosion of hybrid fibre composites

  • M.A. French
  • , G. Pritchard

Research output: Contribution to journalArticlepeer-review

Original languageEnglish
Pages (from-to)257-263
JournalComposites Science and Technology
Volume45
Issue number3
DOIs
Publication statusPublished - 1992
Externally publishedYes

Keywords

  • environmental
  • strain
  • corrosion
  • hybrid
  • epoxy
  • laminate
  • glass
  • carbon
  • diffusion
  • fracture
  • e-glass filaments
  • Chemical engineering